A correlation of the adsorption capacity of perovskite/biochar composite with the metal ion characteristics
Résumé
Abstract LaFeO3/biochar composite is prepared by cellulose-modified microwave-assisted method at 450 °C. The structure is identified by Raman spectrum which, consists of characteristics biochar bands and octahedral perovskite chemical shifts. The morphology is examined by scanning electron microscope (SEM); two phases are observed, rough microporous biochar and orthorhombic perovskite particles. The BET surface area of the composite is 57.63 m2/g. The prepared composite is applied as a sorbent for the removal of Pb2+, Cd2+, and Cu2+ions from aqueous solutions and wastewater. The adsorption ability reaches a maximum at pH > 6 for Cd2+, and Cu2+ions, and is pH-independent for Pb2+ions adsorption. The adsorption follows pseudo 2nd order kinetic model, Langmuir isotherm for Pb2+ions, and Temkin isotherms for Cd2+, and Cu2+ions. The maximum adsorption capacities,qm, are 606, 391, and 112 mg/g for Pb2+, Cd2+, and Cu2+ions, respectively. The electrostatic interaction is responsible for the adsorption of Cd2+, and Cu2+ions on LaFeO3/biochar composite. In case of Pb2+ions form a complex with the surface functional groups of the adsorbate. LaFeO3/biochar composite shows high selectivity for the studied metal ions and excellent performance in real samples. The proposed sorbent can be easily regenerated and effectively reused.
Citer ce document
Exporter : BibTeX · RIS (Zotero, Mendeley, EndNote)
Accès au document
Texte intégral archivé sur SPHAERO, en accès ouvert : lisible gratuitement en ligne après connexion. Le document reste aussi disponible à sa source. Se connecter
Voir l'article sur le site de la revueLicence et provenance
Licence : CC BY
Notice moissonnée depuis OpenAlex le 26/09/2026. Le document reste hébergé par sa source.
Voir le document à la source →