Abstract Antimicrobial and antifungal materials we prepared from Zn-containing wollastonite set by wet precipitation method. Wollastonite, hardystonite, willemite and very little quartz were developed after sintering at 1100°C/2h, however, the Raman spectroscopy approved the later phases by their characteristic Raman shift bands. The microstructure exhibited accumulated rounded to irregular clusters containing nano-size particles (< 500nm) developed in all sintered samples. Zeta potential; exposed negative values for all powdered samples from − 2.64 to -17.6 mV (i.e., for Zn-free to highest Zn-containing samples). It can be easily noticed that the lowest ZnO-content exhibits a varied range of antibacterial activities in contrast to Gram-negative (E. coli) and Gram-positive (S. aureus & B. subtilis). Correspondingly, the CZS5 exhibits good inhibitory effect against the filamentous pathogenic fungus (A. niger).
Citer ce document
Exporter : BibTeX · RIS (Zotero, Mendeley, EndNote)
Accès au document
Texte intégral archivé sur SPHAERO, en accès ouvert : lisible gratuitement en ligne après connexion. Le document reste aussi disponible à sa source. Se connecter
Voir l'article sur le site de la revueLicence et provenance
Licence : CC BY
Notice moissonnée depuis OpenAlex le 10/09/2026. Le document reste hébergé par sa source.
Voir le document à la source →